Röchling SUSTARIN® H

Technical data sheet SUSTARIN H Acetal Homopolymer Delrin ASTM Test method Unit Value Specific Gravity D792 gcm3 1.42 Water Absorption 24 hours D570 0.2 Water Absorption Saturation D570 0.7 Dissipation Factor D150 1 MHz - Hardness D785 Shore D D78 Rockwell Hardness D785 M M85 Rockwell Hardness D785 R R115 Tensile Strength at yield 73 F D638 psi 15000 Tensile Modulus D638 psi 420000 Elongation at Break D638 40 Flexural Strength D790 psi 12000 Flexural Modulus D790 psi 400000 Compressive Strength D695 psi 16000 Shear Strength D732 psi 9000 Izod Impact Notched D256 ft-lbin 1.2 Coefficient of Friction Dynamic - - 0.12 CTE linear D696 ininF 6.7x10-5 Melting Point D3418 F 347 Continuous Use - F 185 Thermal Conductivity - inhrft2F 2 Deflection Temperature at 1.8Mpa 66psi D648 F 290 Deflection Temperature at 1.8Mpa 264psi D648 F 242 Flammability UL94 - inch HB Dielectric constant D150 - 3.1 Surface resistivity D257 Ohmcm 1016 Dielectric strength D149 Vmil 400 - - Yes Physical Properties Mechanical Properties Thermal properties Electrical properties Compliance Properties FDA The data stated above are average values ascertained by statistical tests on a regular basis. The data above are provided purely for information and shall not be regarded as binding unless expressly agreed in a contract of sale. Rchling Engineering Plastics 903 Gastonia Technology Parkway Dallas NC 28034 USA - Tel.704 922 7814 inforoechling-plastics.us www.roechling-plastics.us Status April 19 2016